Título: | NANOSCALE MECHANICAL DEFORMATION MECHANISMS OF POLAR AND NON-POLAR ZNO | ||||||||||||
Autor: |
ELIZANDRA MARTINS SILVA |
||||||||||||
Colaborador(es): |
RODRIGO PRIOLI MENEZES - Orientador |
||||||||||||
Catalogação: | 17/JUN/2015 | Língua(s): | PORTUGUESE - BRAZIL |
||||||||||
Tipo: | TEXT | Subtipo: | THESIS | ||||||||||
Notas: |
[pt] Todos os dados constantes dos documentos são de inteira responsabilidade de seus autores. Os dados utilizados nas descrições dos documentos estão em conformidade com os sistemas da administração da PUC-Rio. [en] All data contained in the documents are the sole responsibility of the authors. The data used in the descriptions of the documents are in conformity with the systems of the administration of PUC-Rio. |
||||||||||||
Referência(s): |
[pt] https://www.maxwell.vrac.puc-rio.br/projetosEspeciais/ETDs/consultas/conteudo.php?strSecao=resultado&nrSeq=24779&idi=1 [en] https://www.maxwell.vrac.puc-rio.br/projetosEspeciais/ETDs/consultas/conteudo.php?strSecao=resultado&nrSeq=24779&idi=2 |
||||||||||||
DOI: | https://doi.org/10.17771/PUCRio.acad.24779 | ||||||||||||
Resumo: | |||||||||||||
In this work, deformation mechanisms of polar and non-polar zinc oxide
(ZnO) were studied by nanoindentation tests. The stable crystal structure of ZnO is
the wurtzite with a strong anisotropic character observed in relation to the
piezoelectricity and spontaneous polarization properties, for example. The
mechanical deformation mechanisms of these sorts of materials are not yet fully
understood, being of vital importance for optoelectronic devices optimization.For
each ZnO crystallographic orientation, the induced defects damages were analyzed
by transmission electron microscopy (TEM) and correlated with the slip of basal
planes {0001} in the divergent directions for the both non-polar faces
(1100) and (1120), as well as for the both polar faces (0001) and (0001). Screw
perfect dislocations were identified by propagating through the slip system (1120)(0001). The beginning of plastic deformation in single crystals is marked by pop-ins events. Such events were identified and analyzed in function of the applied force and size. The residual impressions topography and shape were analyzed by atomic force microscopy (AFM). The observed defects on the surface were
propagated in a preferred direction induced by stress components around the
indentation. Tensile stress generation in a certain direction increases the
dislocations mobility, while compressive stress contributes to pinning regions.
Stress components were identified and their magnitudes were estimated by cathode luminescence method. The polar face (0001) showed a reactive behavior; some defects produced underneath the surface were revealed by samples cleaning process.
|
|||||||||||||
|